I have built the CLC Annapolis Wherry.
The bottom 2 boards outside are covered with fiberglass as are the inside 4
bottom boards.
The clinker ply is joined with epoxy and silica.
It was my first boat and took a long time to sand my over application of
epoxy.
That means tape the inside of the clinker ply joints before expoying.
I could built the a second boat in one fifth the time to took for the first.
Earl